Microstructural and surface analysis of NiTi TPMS lattice sections fabricated by laser powder bed fusion


Journal article


Shahadat Hussain, Alireza Alagha, G. Haidemenopoulos, W. Zaki
Journal of Manufacturing Processes, 2023

Semantic Scholar DOI
Cite

Cite

APA   Click to copy
Hussain, S., Alagha, A., Haidemenopoulos, G., & Zaki, W. (2023). Microstructural and surface analysis of NiTi TPMS lattice sections fabricated by laser powder bed fusion. Journal of Manufacturing Processes.


Chicago/Turabian   Click to copy
Hussain, Shahadat, Alireza Alagha, G. Haidemenopoulos, and W. Zaki. “Microstructural and Surface Analysis of NiTi TPMS Lattice Sections Fabricated by Laser Powder Bed Fusion.” Journal of Manufacturing Processes (2023).


MLA   Click to copy
Hussain, Shahadat, et al. “Microstructural and Surface Analysis of NiTi TPMS Lattice Sections Fabricated by Laser Powder Bed Fusion.” Journal of Manufacturing Processes, 2023.


BibTeX   Click to copy

@article{shahadat2023a,
  title = {Microstructural and surface analysis of NiTi TPMS lattice sections fabricated by laser powder bed fusion},
  year = {2023},
  journal = {Journal of Manufacturing Processes},
  author = {Hussain, Shahadat and Alagha, Alireza and Haidemenopoulos, G. and Zaki, W.}
}


Share


Text Only Owlstown
QR Code
Translate to